Hardox 450 Equivalent: BRINAR® 450

BRINAR® 450 from the Salzgitter Group is comparable in nominal hardness to Hardox® 450 by SSAB. Both grades offer ~450 HB Brinell hardness for severe wear applications. Below we compare their published properties.

Property comparison

PropertyBRINAR® 450Hardox® 450
ManufacturerIlsenburger Grobblech (Salzgitter AG), AlemaniaSSAB, Suecia / Finlandia
Nominal hardness420–470 HB~450 HB (range per SSAB datasheet)
Yield strength1100 MPa—
Tensile strength1350 MPa—
Impact energy40 J (-20°C)—
Max thickness100 mm—
Material number1.8722—

Equivalency is based on nominal hardness; it does not imply identical chemical composition, heat treatment or properties. BRINAR® data is from official Salzgitter datasheets. Hardox® data will be completed from SSAB's public datasheet. Hardox® is a registered trademark of SSAB.

When are they interchangeable?

In applications where the primary requirement is surface hardness (~450 HB), BRINAR® 450 and Hardox® 450 can be functionally interchangeable. This includes wear liners, hoppers, chutes and crusher components.

However, differences in exact chemical composition, manufacturing process and tolerances may make one grade more suitable than the other in applications requiring specific welding, cold forming or particular certifications. Always consult the technical datasheets from both manufacturers.

Advantages of BRINAR® in Mexico

  • ✓German manufacturing: produced by Ilsenburger Grobblech GmbH (Salzgitter Group), with over 130 years of experience.
  • ✓Warehouse in Mexico: available in stock in Cd. Benito Juárez, Nuevo León, through AAMSA.
  • ✓Complete documentation: material test report (MTR) and per-plate traceability.
  • ✓SALCOS low-CO₂ green steel option available.

Need a Hardox® 450 equivalent?

Quote BRINAR® 450 with delivery from our warehouse in Monterrey.

Get a quote