Material number: 1.8722

BRINAR® 450 Wear Plate (AR450 · 450 HB)

German manufacturing by the Salzgitter Group · Available in stock in Nuevo León, Mexico

BRINAR® 450 is a wear-resistant steel plate with a nominal hardness of 450 HB, designed for more severe abrasion conditions than those handled by grade 400. It combines high hardness with adequate toughness, providing longer service life in mining and heavy industry applications.

With material number 1.8722 and available thicknesses up to 100 mm, BRINAR® 450 is produced through controlled quenching and tempering that guarantees hardness uniformity throughout the thickness. Its yield point of 1 100 MPa and tensile strength of 1 350 MPa position it as a high-performance solution for equipment subjected to combined abrasive loads and impacts.

BRINAR® 450 wear-resistant steel plate

450 HB

Nominal hardness

1 350 MPa

Tensile strength

40 J

Impact energy (−20°C)

100 mm

Maximum thickness

Chemical composition (% by mass, max.)

CSiMnPSCrMoNiBAl
0.260.61.50.0180.0051.80.652.10.0050.1

Ti and/or V and/or Nb may additionally be present as microalloying elements.

Mechanical properties (reference 20 mm)

Hardness (HB)Yield point (MPa)Tensile strength (MPa)Elongation (%)Impact energy (J, -20°C)
44011001350940

Guaranteed hardness range

Minimum (HB)Maximum (HB)Note
420470–

Available dimensions

Maximum thickness: 100 mm. Widths and lengths per EN 10029.

Grade equivalences

BRINAR® (Salzgitter)AR (ASTM)NM (Chinese)Hardox® (SSAB)
BRINAR® 450AR450NM450Hardox® 450

Equivalency is based on nominal hardness; it does not imply identical chemical composition, heat treatment or properties. Hardox® is a registered trademark of SSAB.

See full equivalence table →

Recommended applications

  • ‣Jaw and cone crusher liners
  • ‣Wear plates on mineral conveyor belts
  • ‣High-tonnage hydraulic excavator buckets
  • ‣Hoppers and gates in mineral processing plants
  • ‣Ball and SAG mill liners
  • ‣Dredging equipment and abrasive rock handling
  • ‣Protection structures on construction machinery

Welding and cutting

BRINAR® 450 can be welded using low-hydrogen basic electrodes. Preheating depends on thickness and ambient temperature. Plasma or oxy-fuel cutting is feasible across all available thicknesses.

For detailed welding procedures, refer to the technical datasheet or our guide (coming soon).

Stock available in Nuevo León, Mexico

Salzgitter Mannesmann International warehouse in Cd. Benito Juárez, Nuevo León. Authorised distributor: AAMSA.

Request a quote

Compare with other BRINAR® grades

BRINAR® 450 is ideal when abrasion is severe but some impact toughness is required. If weldability is a priority and wear is moderate, BRINAR® 400 is more suitable. For purely abrasive wear with very hard minerals, BRINAR® 500 is the choice.

Frequently asked questions about BRINAR® 450

What is the difference between BRINAR® 450 and BRINAR® 400 in terms of hardness and wear resistance?

BRINAR® 450 offers a guaranteed hardness of 420–470 HB versus the 370–440 HB range of BRINAR® 400. In general, higher hardness means higher abrasion resistance; BRINAR® 450 can deliver up to 15–20 % longer service life in pure wear applications. The trade-off is lower elongation (9 % vs 12 %) and lower impact energy (40 J vs 60 J).

What are the preheat recommendations for welding BRINAR® 450?

Due to its higher carbon equivalent (CEV of 0.48 at 15 mm), BRINAR® 450 requires more careful preheating than grade 400. Preheating between 125 °C and 175 °C depending on thickness is recommended, using low-hydrogen basic electrodes and avoiding rapid cooling after welding. Consult the manufacturer's technical datasheet for detailed procedures.

Is BRINAR® 450 suitable for applications with strong and frequent impacts?

BRINAR® 450 exhibits an impact energy of 40 J at −20°C, giving it adequate toughness for moderate impacts. In applications with very severe and frequent impacts, it should be evaluated whether BRINAR® 400 (60 J) would be more appropriate, as higher toughness can prevent brittle fracture. For dominant wear with moderate impact, BRINAR® 450 is the optimal choice.

What market steels are equivalent to BRINAR® 450?

BRINAR® 450 is comparable in hardness range to Hardox® 450 (SSAB), Dillidur 450V (Dillinger), XAR® 450 (ThyssenKrupp) and Creusabro® 4800 (Industeel). Each manufacturer has its own chemical composition specification and manufacturing process, so properties may vary slightly. BRINAR® production at Ilsenburg (Germany) guarantees Salzgitter Group quality.

In what thicknesses is BRINAR® 450 available and what is the delivery lead time in Mexico?

BRINAR® 450 is available in thicknesses up to 100 mm. Inventory in Mexico is maintained at the warehouse in Cd. Benito Juárez, Nuevo León, distributed by Salzgitter Mannesmann International and its authorised distributor AAMSA. Delivery lead times depend on thickness and availability; contact the sales team to check current stock and timelines.

MAXIL®

Need high-strength structural steel? Discover MAXIL®, also from the Salzgitter Group.

Explore MAXIL® →

Applications where BRINAR® 450 is used