Hardox 400 Equivalent: BRINAR® 400

BRINAR® 400 from the Salzgitter Group is comparable in nominal hardness to Hardox® 400 by SSAB. Both grades offer ~400 HB Brinell hardness for severe wear applications. Below we compare their published properties.

Property comparison

PropertyBRINAR® 400Hardox® 400
ManufacturerIlsenburger Grobblech (Salzgitter AG), AlemaniaSSAB, Suecia / Finlandia
Nominal hardness370–440 HB~400 HB (range per SSAB datasheet)
Yield strength960 MPa—
Tensile strength1200 MPa—
Impact energy60 J (-20°C)—
Max thickness120 mm—
Material number1.8714—

Equivalency is based on nominal hardness; it does not imply identical chemical composition, heat treatment or properties. BRINAR® data is from official Salzgitter datasheets. Hardox® data will be completed from SSAB's public datasheet. Hardox® is a registered trademark of SSAB.

When are they interchangeable?

In applications where the primary requirement is surface hardness (~400 HB), BRINAR® 400 and Hardox® 400 can be functionally interchangeable. This includes wear liners, hoppers, chutes and crusher components.

However, differences in exact chemical composition, manufacturing process and tolerances may make one grade more suitable than the other in applications requiring specific welding, cold forming or particular certifications. Always consult the technical datasheets from both manufacturers.

Advantages of BRINAR® in Mexico

  • ✓German manufacturing: produced by Ilsenburger Grobblech GmbH (Salzgitter Group), with over 130 years of experience.
  • ✓Warehouse in Mexico: available in stock in Cd. Benito Juárez, Nuevo León, through AAMSA.
  • ✓Complete documentation: material test report (MTR) and per-plate traceability.
  • ✓SALCOS low-CO₂ green steel option available.

Need a Hardox® 400 equivalent?

Quote BRINAR® 400 with delivery from our warehouse in Monterrey.

Get a quote