Material number: 1.8714
BRINAR® 400 Wear Plate (AR400 · 400 HB)
German manufacturing by the Salzgitter Group · Available in stock in Nuevo León, Mexico
BRINAR® 400 is a wear-resistant steel plate with a nominal hardness of 400 HB, produced by the Salzgitter Group in Germany. It provides an outstanding balance between abrasion resistance, toughness and weldability, making it the preferred choice for applications that combine moderate impact with severe wear.
With material number 1.8714 and available thicknesses up to 120 mm, BRINAR® 400 is manufactured through a controlled rolling and direct quenching process that ensures a homogeneous martensitic microstructure throughout the cross-section. Its optimised chemical composition with Cr, Mo, Ni and B delivers superior mechanical properties with a tensile strength of 1 200 MPa and an impact energy of 60 J at −20°C.

400 HB
Nominal hardness
1 200 MPa
Tensile strength
60 J
Impact energy (−20°C)
120 mm
Maximum thickness
Chemical composition (% by mass, max.)
| C | Si | Mn | P | S | Cr | Mo | Ni | B | Al |
|---|---|---|---|---|---|---|---|---|---|
| 0.3 | 0.6 | 1.5 | 0.018 | 0.005 | 1.8 | 0.6 | 2.1 | 0.005 | 0.1 |
Ti and/or V and/or Nb may additionally be present as microalloying elements.
Mechanical properties (reference 20 mm)
| Hardness (HB) | Yield point (MPa) | Tensile strength (MPa) | Elongation (%) | Impact energy (J, -20°C) |
|---|---|---|---|---|
| 400 | 960 | 1200 | 12 | 60 |
Guaranteed hardness range
| Minimum (HB) | Maximum (HB) | Note |
|---|---|---|
| 370 | 440 | – |
Available dimensions
Maximum thickness: 120 mm. Widths and lengths per EN 10029.
Grade equivalences
| BRINAR® (Salzgitter) | AR (ASTM) | NM (Chinese) | Hardox® (SSAB) |
|---|---|---|---|
| BRINAR® 400 | AR400 | NM400 | Hardox® 400 |
Equivalency is based on nominal hardness; it does not imply identical chemical composition, heat treatment or properties. Hardox® is a registered trademark of SSAB.
See full equivalence table →Recommended applications
- ‣Mining machinery buckets and hoppers
- ‣Dump truck bodies
- ‣Crushers and mills
- ‣Earthmoving equipment
- ‣Mineral transport chutes and ducts
- ‣Bunker and silo linings
- ‣Heavy-duty agricultural and industrial equipment
Welding and cutting
BRINAR® 400 can be welded using low-hydrogen basic electrodes. Preheating depends on thickness and ambient temperature. Plasma or oxy-fuel cutting is feasible across all available thicknesses.
For detailed welding procedures, refer to the technical datasheet or our guide (coming soon).
Stock available in Nuevo León, Mexico
Salzgitter Mannesmann International warehouse in Cd. Benito Juárez, Nuevo León. Authorised distributor: AAMSA.
Compare with other BRINAR® grades
BRINAR® 400 is the best choice when a balance between wear resistance and weldability is needed. For more severe abrasion with less impact, consider BRINAR® 450. For the most extreme pure wear conditions, BRINAR® 500 offers maximum hardness.
Frequently asked questions about BRINAR® 400
What hardness does BRINAR® 400 guarantee and how is it verified?
BRINAR® 400 guarantees a hardness of 370–440 HB in accordance with EN 10029. The typical value on a 20 mm plate is 400 HB. Hardness is measured with a Brinell hardness tester directly on the plate surface after light surface preparation.
Can BRINAR® 400 be welded without preheating?
Thanks to its low carbon equivalent (CEV of 0.41 at 15 mm), BRINAR® 400 can be welded without preheat on thin gauges under controlled conditions. For greater thicknesses or low ambient temperatures, preheating to 100 °C–150 °C and the use of low-hydrogen basic electrodes are recommended.
In which industrial applications is BRINAR® 400 most suitable?
BRINAR® 400 is especially suited for applications combining abrasive wear with moderate impact: mining buckets, dump truck bodies, ore chutes, crushers and earthmoving equipment liners. Its higher elongation (12 %) compared to higher grades makes it more tolerant to dynamic loads.
What are the international equivalents of BRINAR® 400?
BRINAR® 400 is comparable in hardness range to Hardox® 400 (SSAB), Dillidur 400V (Dillinger), XAR® 400 (ThyssenKrupp) and Creusabro® 4000 (Industeel). However, the exact chemical composition and mechanical properties may vary between manufacturers; always consult the technical datasheets for a precise comparison.
In what thicknesses and formats is BRINAR® 400 available in Mexico?
BRINAR® 400 is distributed in Mexico through Salzgitter Mannesmann International with inventory in Cd. Benito Juárez, Nuevo León. Available thicknesses range from 6 mm to 120 mm in plates of standard widths and lengths. For special requirements or custom orders, contact the sales team directly.
MAXIL®