Material number: 1.8734
BRINAR® 500 Wear Plate (AR500 · 500 HB)
German manufacturing by the Salzgitter Group · Available in stock in Nuevo León, Mexico
BRINAR® 500 is the highest-hardness wear-resistant steel plate in the BRINAR® range, with a nominal hardness of 500 HB. It is designed for the most extreme abrasion conditions, where maximum wear resistance is the primary requirement and component weight and cost must be minimised.
With material number 1.8734 and available thicknesses up to 80 mm, BRINAR® 500 is produced through a high-precision direct rolling and quenching process. Its tensile strength of 1 500 MPa and yield point of 1 300 MPa make this grade the optimal choice for wear components exposed to highly abrasive minerals such as silica, basalt or granite.

500 HB
Nominal hardness
1 500 MPa
Tensile strength
30 J
Impact energy (−20°C)
80 mm
Maximum thickness
Chemical composition (% by mass, max.)
| C | Si | Mn | P | S | Cr | Mo | Ni | B | Al |
|---|---|---|---|---|---|---|---|---|---|
| 0.32 | 0.8 | 1.5 | 0.018 | 0.005 | 1.8 | 0.65 | 2.1 | 0.005 | 0.1 |
Ti and/or V and/or Nb may additionally be present as microalloying elements.
Mechanical properties (reference 20 mm)
| Hardness (HB) | Yield point (MPa) | Tensile strength (MPa) | Elongation (%) | Impact energy (J, -20°C) |
|---|---|---|---|---|
| 490 | 1300 | 1500 | 7 | 30 |
Guaranteed hardness range
| Minimum (HB) | Maximum (HB) | Thickness condition |
|---|---|---|
| 470 | 540 | Plates with thickness ≤ 30 mm |
| 450 | 540 | Plates with thickness > 30 mm |
Available dimensions
Maximum thickness: 80 mm. Widths and lengths per EN 10029.
Grade equivalences
| BRINAR® (Salzgitter) | AR (ASTM) | NM (Chinese) | Hardox® (SSAB) |
|---|---|---|---|
| BRINAR® 500 | AR500 | NM500 | Hardox® 500 |
Equivalency is based on nominal hardness; it does not imply identical chemical composition, heat treatment or properties. Hardox® is a registered trademark of SSAB.
See full equivalence table →Recommended applications
- ‣Crusher liners exposed to basalt, granite and silica
- ‣Bucket teeth and lips in open-pit mining
- ‣Scraper and deflector plates on high-speed conveyors
- ‣Coke and slag hoppers and gates
- ‣Hard-rock drilling equipment wear components
- ‣Cement and fly-ash silo liners
- ‣Wear parts in metal recycling facilities
Welding and cutting
BRINAR® 500 can be welded using low-hydrogen basic electrodes. Preheating depends on thickness and ambient temperature. Plasma or oxy-fuel cutting is feasible across all available thicknesses.
For detailed welding procedures, refer to the technical datasheet or our guide (coming soon).
Stock available in Nuevo León, Mexico
Salzgitter Mannesmann International warehouse in Cd. Benito Juárez, Nuevo León. Authorised distributor: AAMSA.
Compare with other BRINAR® grades
BRINAR® 500 is the choice when abrasive wear is extreme and impact is low. For applications with moderate impact, BRINAR® 450 offers better toughness. If maximum weldability is required, BRINAR® 400 is the most versatile grade.
Frequently asked questions about BRINAR® 500
What is the guaranteed hardness range for BRINAR® 500 and does it vary with thickness?
Yes, the hardness range of BRINAR® 500 depends on plate thickness. For thicknesses up to and including 30 mm, the guaranteed range is 470–540 HB. For thicknesses above 30 mm, the range broadens to 450–540 HB. The typical value on a 20 mm plate is 490 HB.
What special considerations are there for welding BRINAR® 500?
BRINAR® 500 is the highest-carbon grade in the range (max. 0.32 %), which demands rigorous control of the welding process. Preheating of 150–200 °C depending on thickness and ambient temperature is required, together with very low-hydrogen basic electrodes (H≤2 ml/100 g), controlled heat input and, preferably, post-weld heat treatment (PWHT) to relieve residual stresses.
In which applications does BRINAR® 500 offer a clear advantage over grades 400 and 450?
BRINAR® 500 excels in purely abrasive wear applications with very hard minerals (quartz, basalt, granite) and low impact load. Its higher hardness (490 HB typical) can result in a 30–50 % increase in service life compared to grade 400 under these conditions. It also allows reducing plate thickness while maintaining the same service life, with the associated weight saving.
What are the international equivalents of BRINAR® 500?
BRINAR® 500 is comparable in hardness range to Hardox® 500 (SSAB), Dillidur 500 (Dillinger) and XAR® 500 (ThyssenKrupp). Each grade presents differences in chemical composition, manufacturing process and guaranteed properties. BRINAR® 500 is produced at the Ilsenburg plant of Ilsenburger Grobblech, part of the Salzgitter Group, guaranteeing European traceability and quality.
Up to what thickness is BRINAR® 500 available and are there cutting or bending restrictions?
BRINAR® 500 is available in thicknesses up to 80 mm. Plasma or oxy-fuel cutting is feasible, although preheating the cutting zone is recommended for greater thicknesses. Regarding bending, minimum radii are larger than for lower grades (r/t of 4.0–5.5 depending on direction and thickness), so high-tonnage presses must be used. For thicknesses above 20 mm, light preheating before bending is recommended.