Wear Plate for Dump Truck Bodies: Selection Guide
Dump truck bodies suffer severe wear on the floor, lower sidewalls and tailgate. BRINAR® 400 (370–440 HB) is the recommended grade for general use due to its balance between abrasion resistance and impact toughness (60 J at −20°C). For operations with extremely abrasive material, BRINAR® 450 (420–470 HB) offers longer service life in critical wear zones.
The wear problem in dump truck bodies
Dump truck bodies are subjected to a combination of abrasive wear and mechanical impact during loading, hauling and dumping. Using conventional structural steel results in short service lives, frequent repair shutdowns and high maintenance costs. BRINAR® wear plate is a proven solution that can multiply component service life.
Critical wear zones
Not all zones in the body experience the same level of wear. The critical areas are:
| Zone | Type of wear | Severity |
|---|---|---|
| Floor (loading zone) | Impact + abrasion | Very high |
| Floor (sliding zone) | Sliding abrasion | High |
| Lower sidewalls | Abrasion + lateral impact | High |
| Upper sidewalls | Light abrasion | Moderate |
| Tailgate | Sliding abrasion | High |
| Front canopy | Direct loading impact | Very high |
Recommended grades
Grade selection depends on the type of material hauled and the severity of the operation:
- BRINAR® 400 (370–440 HB): Recommended for general use. Its impact energy of 60 J at −20°C and 12% elongation make it ideal for zones receiving direct impact during loading. Yield point of 960 MPa and tensile strength of 1,200 MPa.
- BRINAR® 450 (420–470 HB): Recommended for severe conditions with highly abrasive materials (iron ore, copper, crushed rock). Can offer 15–20% longer service life than grade 400 in pure abrasion, at the cost of lower toughness (40 J) and elongation (9%).
For specific thickness recommendations per zone, consult the BRINAR® technical team, as it depends on truck tonnage, material type and loading cycle frequency.
Typical dump truck body configuration
An optimised configuration can combine grades in different zones:
- Floor loading and impact zone: BRINAR® 400 for maximum toughness
- Floor sliding zone: BRINAR® 400 or 450 depending on severity
- Lower sidewalls: BRINAR® 400
- Upper sidewalls: Structural steel or BRINAR® 400 in reduced thickness
- Tailgate: BRINAR® 400 or 450
- Front canopy: BRINAR® 400 (maximum impact)
Benefits vs conventional structural steel
- Longer service life: The hardness of BRINAR® 400 (370–440 HB) is 2x to 3x that of common structural steel (120–160 HB), multiplying service life.
- Weight reduction: Being more resistant, thinner gauges can be used for the same service life, reducing body dead weight and increasing payload.
- Lower cost per tonne hauled: The combination of longer service life and higher payload significantly reduces operating cost per tonne.
- Fewer maintenance stops: Fewer plate changes means greater equipment availability.
Weldability in body fabrication
BRINAR® 400 has a CEV of 0.41 at 15 mm, which facilitates welding with minimal preheat at thicknesses typical for dump truck bodies. Low-hydrogen basic electrodes and controlled heat input are recommended to preserve hardness in the heat-affected zone.
For more information on welding, see our dedicated guide.
Frequently asked questions
Which wear-resistant steel grade is best for dump truck bodies?
BRINAR® 400 is the most recommended grade for dump truck bodies due to its balance between abrasion resistance (370–440 HB) and impact toughness (60 J at −20°C). For operations with extremely abrasive material and low impact, BRINAR® 450 may offer longer service life.
What are the highest-wear zones in a dump truck body?
The highest-wear zones are the floor in the loading zone (impact + abrasion), the front canopy (direct impact) and the tailgate (sliding abrasion). The lower sidewalls also experience significant wear from abrasion and lateral impact.
How much longer does a dump truck body last with wear plate vs structural steel?
The hardness of BRINAR® 400 (370–440 HB) is 2x to 3x that of conventional structural steel (120–160 HB). In practice, this can translate to 2 to 4 times longer service life depending on the hauled material and operating conditions.
Can BRINAR® 400 be welded for dump truck body fabrication?
Yes. BRINAR® 400 has a CEV of 0.41 at 15 mm thickness, allowing welding with minimal preheat at thicknesses typical for dump truck bodies. Low-hydrogen basic electrodes and controlled heat input are required.
Related grades
Need wear-resistant steel for your project?
Quote BRINAR® 400, 450 or 500 with delivery from our warehouse in Monterrey.