Brinell Hardness: What It Is, How It Is Measured and Its Relation to Wear-Resistant Steel
Brinell hardness (HB) is a scale that measures a material's resistance to permanent indentation. The test uses a 10 mm diameter tungsten carbide ball with a 3,000 kgf (29.42 kN) load. It is the industry standard for wear-resistant steel because the impression covers a representative area of the microstructure. BRINAR® grades map directly to the scale: 400 = 370–440 HB, 450 = 420–470 HB, 500 = 470–540 HB.
What is Brinell hardness
Brinell hardness is a measure of a material's resistance to localised plastic deformation caused by a load applied through a spherical indenter. It was proposed by Swedish engineer Johan August Brinell in 1900 and has become the reference method for evaluating the hardness of wear-resistant steels worldwide.
The Brinell hardness value is expressed in HBW (Hardness Brinell Tungsten carbide) and represents the ratio between the applied force and the area of the impression left by the ball on the material surface.
How the Brinell test works
The test is performed following ISO 6506 (equivalent to ASTM E10) with the following standard parameters for steels:
| Parameter | Standard value |
|---|---|
| Indenter | Tungsten carbide (WC) ball |
| Ball diameter | 10 mm |
| Test load | 3,000 kgf (29.42 kN) |
| Load application time | 10–15 seconds |
| Load/diameter² ratio | 30 (for steels) |
The procedure consists of: (1) preparing the material surface by removing rust and irregularities, (2) applying the load through the ball for the specified time, (3) removing the load, and (4) measuring the diameter of the residual impression with a microscope. The HBW value is calculated from the force, ball diameter and impression diameter.
Why Brinell hardness is the standard for wear-resistant steel
Brinell hardness has specific advantages that make it ideal for wear-resistant steels:
- Large, representative impression: The 10 mm ball generates an impression several millimetres in diameter, averaging hardness over a significant area of the microstructure. This is crucial in quenched steels where local variations may exist.
- Method robustness: The test is less sensitive to surface preparation than other methods (Vickers, Rockwell), making it practical for plant and field measurements.
- Direct correlation with wear resistance: There is a well-documented relationship between Brinell hardness and abrasion resistance. In general, higher HB means longer service life under wear conditions.
- Established industry standard: Wear-resistant steel manufacturers worldwide specify their products in HBW, facilitating comparison between brands.
Brinell hardness of BRINAR® grades
The numerical designation of BRINAR® grades corresponds directly to their nominal Brinell hardness:
| Grade | Nominal hardness (HB) | Guaranteed range (HB) | Typical value at 20 mm (HB) |
|---|---|---|---|
| BRINAR® 400 | 400 | 370–440 | 400 |
| BRINAR® 450 | 450 | 420–470 | 440 |
| BRINAR® 500 | 500 | 470–540 (≤30 mm) / 450–540 (>30 mm) | 490 |
The guaranteed range ensures that every plate delivered meets the specified hardness. Variation within the range is due to normal differences in thickness and position on the plate.
Relationship between Brinell hardness and wear resistance
The relationship between hardness and wear resistance is not linear, but it is consistent: a hardness increase from 400 HB to 500 HB can represent 30% to 50% longer service life under pure sliding abrasion conditions. However, this relationship changes when impact is involved, as higher hardness comes with lower toughness.
Therefore, grade selection should not be based solely on the highest available hardness, but on the optimal balance between wear resistance and toughness for the specific operating conditions.
Other hardness scales
There are other hardness scales used in industry:
- Rockwell C (HRC): Uses a diamond cone. Approximate conversion: 400 HB ≈ 42 HRC, 450 HB ≈ 47 HRC, 500 HB ≈ 51 HRC. Frequently used in heat treatment but its smaller impression makes it less representative for thick plates.
- Vickers (HV): Uses a diamond pyramid. Values are numerically similar to HB in the wear-resistant steel range. Mainly used in laboratory and for microstructures.
For wear-resistant steel in plate format, Brinell hardness remains the reference method for the reasons mentioned above.
Frequently asked questions
What does the number in wear-resistant steel grades (400, 450, 500) mean?
The number indicates the nominal Brinell hardness of the steel. BRINAR® 400 has a nominal hardness of 400 HB (guaranteed range 370–440 HB), BRINAR® 450 of 450 HB (420–470 HB) and BRINAR® 500 of 500 HB (470–540 HB).
How is Brinell hardness measured on a steel plate?
A 10 mm diameter tungsten carbide ball is used with a 3,000 kgf load applied for 10–15 seconds. The diameter of the residual impression is measured with a microscope and the HBW value is calculated. The test follows ISO 6506.
Does higher Brinell hardness mean greater wear resistance?
Generally yes: an increase from 400 to 500 HB can represent 30–50% longer service life under sliding abrasion. However, higher hardness also means lower impact toughness, so in applications with significant impact, a softer grade may offer better overall performance.
What is the difference between Brinell and Rockwell hardness?
Brinell hardness (HBW) uses a 10 mm ball and generates a large, representative impression, ideal for thick plates. Rockwell C hardness (HRC) uses a diamond cone with a much smaller impression. Approximate conversion: 400 HB ≈ 42 HRC, 450 HB ≈ 47 HRC, 500 HB ≈ 51 HRC.
Related grades
Need wear-resistant steel for your project?
Quote BRINAR® 400, 450 or 500 with delivery from our warehouse in Monterrey.