Wear Plate Service Life and Cost Savings
How to calculate BRINAR® wear plate service life and cost savings vs structural steel in mining and industrial applications.

How long does a wear plate last?
The service life of a wear plate depends on several factors: mineral type (hardness, particle shape, size), contact speed, impact angle, temperature and the presence of moisture or corrosive agents.
As a general rule, when switching from structural steel S355 (~150 HB) to BRINAR® 400 (~400 HB), service life is multiplied by a factor of 2 to 4 under sliding abrasion conditions. In impact abrasion, the factor is lower (1.5 to 2.5) because toughness also plays a role.
How to estimate savings
The savings calculation considers:
- Plate cost — BRINAR® has a higher price per kg than structural steel, but less thickness is needed.
- Installation cost — labour for plate change, welding, cutting.
- Downtime cost — each plate change requires stopping the equipment. Longer life = fewer stops.
- Weight savings — in dump truck bodies, lower weight = more payload per trip = more tonnes hauled per shift.
Simplified example
If an S355 plate of 25 mm lasts 6 months in a bucket, a BRINAR® 400 plate of 20 mm can last 18–24 months under the same conditions. The additional cost of BRINAR® is recovered in the first avoided replacement cycle.
Factors affecting service life
| Factor | Effect |
|---|---|
| Mineral hardness | Harder mineral = more wear |
| Particle size | Large particles = more impact; fine = more abrasion |
| Contact speed | Higher speed = exponentially more wear |
| Impact angle | 90° = maximum impact; 15–30° = maximum abrasion |
| Moisture and corrosion | Accelerate wear, especially with acidic minerals |