Choosing the right wear plate requires evaluating specific operating conditions. There is no universal grade — each application has different demands.

1. Type of wear

Identify the predominant wear mechanism:

  • Sliding abrasion: Fine material sliding over the surface. Favors higher hardness grades (450–500 HB).
  • Impact abrasion: Blows from coarse material or rocks. Requires toughness, favoring intermediate grades (400–450 HB).
  • Combined abrasion: Most mining applications. Evaluate which mechanism predominates.

2. Required thickness

Thickness depends on desired service life and available space. As reference:

  • Dump truck bodies: 6–16 mm
  • Buckets: 16–40 mm
  • Crushers: 25–80 mm
  • Transfer chutes: 10–25 mm

3. Weldability

Higher hardness means more caution when welding. BRINAR® 400 can be welded with minimal preheating (75–100°C), while 500 requires stricter procedures (150–200°C preheating).

4. Operating temperature

Quenched and tempered steels lose hardness at elevated temperatures. For applications above 250°C, consult the technical data sheets for each grade.

Quick reference table

Use this table as a starting point, and consult with our technical team for a recommendation specific to your project.

Need wear-resistant steel for your project?

Quote BRINAR® 400, 450 or 500 with delivery from our warehouse in Monterrey.

Get a quote