Technical Guide

Hardox, AR and NM Equivalents Explained

Understand the equivalences between Hardox, AR400/AR450/AR500, NM400/NM450/NM500 and BRINAR® by nominal Brinell hardness.

Hardox, AR and NM Equivalents Explained

What do the Hardox, AR and NM designations mean?

In the wear-resistant steel market, there are multiple designations that can cause confusion. The three most common are:

  • AR (Abrasion Resistant) — North American designation (ASTM A514) followed by the hardness level: AR400, AR450, AR500.
  • NM (Nai Mo, 耐磨) — Chinese designation (GB/T 24186) meaning "wear-resistant": NM400, NM450, NM500.
  • Hardox® — Trade name by SSAB (Sweden/Finland): Hardox 400, 450, 500.
  • BRINAR® — Trade name by the Salzgitter Group (Germany): BRINAR 400, 450, 500.

Equivalence table by nominal hardness

HardnessBRINAR® (Salzgitter)Hardox® (SSAB)AR (ASTM)NM (Chinese)
~400 HBBRINAR® 400Hardox® 400AR400NM400
~450 HBBRINAR® 450Hardox® 450AR450NM450
~500 HBBRINAR® 500Hardox® 500AR500NM500

Are they really the same?

No. Equivalency is based on nominal hardness, but each manufacturer has its own chemical composition, manufacturing process and guaranteed property ranges. For example, BRINAR® 400 guarantees 370–440 HB with a yield strength of 960 MPa and impact energy of 60 J at −20°C. Other manufacturers may have different ranges.

For this reason, when substituting one brand for another, the full technical datasheet should be compared, not just hardness.

Why choose BRINAR®?

BRINAR® offers German manufacturing (Ilsenburger Grobblech, Salzgitter Group), certified documentation (MTR), availability in stock in Mexico and the SALCOS low-CO₂ green steel option.

Need wear-resistant steel for your project?

Quote BRINAR® 400, 450 or 500 with delivery from our warehouse in Monterrey.