What do the Hardox, AR and NM designations mean?
In the wear-resistant steel market, there are multiple designations that can cause confusion. The three most common are:
- AR (Abrasion Resistant) — North American designation (ASTM A514) followed by the hardness level: AR400, AR450, AR500.
- NM (Nai Mo, 耐磨) — Chinese designation (GB/T 24186) meaning "wear-resistant": NM400, NM450, NM500.
- Hardox® — Trade name by SSAB (Sweden/Finland): Hardox 400, 450, 500.
- BRINAR® — Trade name by the Salzgitter Group (Germany): BRINAR 400, 450, 500.
Equivalence table by nominal hardness
| Hardness | BRINAR® (Salzgitter) | Hardox® (SSAB) | AR (ASTM) | NM (Chinese) |
|---|---|---|---|---|
| ~400 HB | BRINAR® 400 | Hardox® 400 | AR400 | NM400 |
| ~450 HB | BRINAR® 450 | Hardox® 450 | AR450 | NM450 |
| ~500 HB | BRINAR® 500 | Hardox® 500 | AR500 | NM500 |
Are they really the same?
No. Equivalency is based on nominal hardness, but each manufacturer has its own chemical composition, manufacturing process and guaranteed property ranges. For example, BRINAR® 400 guarantees 370–440 HB with a yield strength of 960 MPa and impact energy of 60 J at −20°C. Other manufacturers may have different ranges.
For this reason, when substituting one brand for another, the full technical datasheet should be compared, not just hardness.
Why choose BRINAR®?
BRINAR® offers German manufacturing (Ilsenburger Grobblech, Salzgitter Group), certified documentation (MTR), availability in stock in Mexico and the SALCOS low-CO₂ green steel option.
Need wear-resistant steel for your project?
Quote BRINAR® 400, 450 or 500 with delivery from our warehouse in Monterrey.