How to choose the right wear plate for your project
Key factors for selecting wear plate grade and thickness: type of abrasion, impact, operating temperature and required weldability.

Selection factors
Choosing the right wear plate requires evaluating specific operating conditions. There is no universal grade — each application has different demands.
1. Type of wear
Identify the predominant wear mechanism:
- Sliding abrasion: Fine material sliding over the surface. Favors higher hardness grades (450–500 HB).
- Impact abrasion: Blows from coarse material or rocks. Requires toughness, favoring intermediate grades (400–450 HB).
- Combined abrasion: Most mining applications. Evaluate which mechanism predominates.
2. Required thickness
Thickness depends on desired service life and available space. As reference:
- Dump truck bodies: 6–16 mm
- Buckets: 16–40 mm
- Crushers: 25–80 mm
- Transfer chutes: 10–25 mm
3. Weldability
Higher hardness means more caution when welding. BRINAR® 400 can be welded with minimal preheating (75–100°C), while 500 requires stricter procedures (150–200°C preheating).
4. Operating temperature
Quenched and tempered steels lose hardness at elevated temperatures. For applications above 250°C, consult the technical data sheets for each grade.
Quick reference table
Use this table as a starting point, and consult with our technical team for a recommendation specific to your project.
Need wear-resistant steel for your project?
Quote BRINAR® 400, 450 or 500 with delivery from our warehouse in Monterrey.